Experimental studies of the defect structure of the TIO 2(110) surface before and after the exposure to oxygen, hydrogen and carbon monoxide

dc.contributor.authorRocker, Gerd Heinrichen
dc.date.accessioned2015-05-12T20:43:17Z
dc.date.available2015-05-12T20:43:17Z
dc.date.issued1985en
dc.identifier.urihttps://scholarworks.montana.edu/handle/1/4528en
dc.language.isoenen
dc.publisherMontana State University - Bozeman, College of Letters & Scienceen
dc.rights.holderCopyright 1985 by Gerd Heinrich Rockeren
dc.subject.lcshTitanium dioxideen
dc.subject.lcshSurface chemistryen
dc.subject.lcshCatalysisen
dc.subject.lcshMetalsen
dc.subject.lcshGasesen
dc.subject.lcshAdsorptionen
dc.titleExperimental studies of the defect structure of the TIO 2(110) surface before and after the exposure to oxygen, hydrogen and carbon monoxideen
dc.typeDissertationen
thesis.catalog.ckey303787en
thesis.degree.departmentPhysics.en
thesis.degree.genreDissertationen
thesis.degree.namePhDen
thesis.format.extentfirstpage1en
thesis.format.extentlastpage284en

Files

Original bundle

Now showing 1 - 1 of 1
Thumbnail Image
Name:
31762100111788.pdf
Size:
10.73 MB
Format:
Adobe Portable Document Format
Copyright (c) 2002-2022, LYRASIS. All rights reserved.